低温用无缝钢管和焊接钢管 ASTM A333.Grade 6低温冲击试验
低温用无缝钢管和焊接钢管 ASTM A333.Grade 6低温冲击试验
低温用无缝钢管和焊接钢管 ASTM A333.Grade 6低温冲击试验
低温用无缝钢管和焊接钢管
标准
ASTM A333——Seamless and Welded Steel Pipe for Low-Temperature Service
主要生产钢管牌号
Grade 1, Grade 3, Grade 4, Grade 6, Grade 7, Grade 8, Grade 9, Grade 10, Grade 11
冲击温度
级别 |
最低冲击试验温度 | |
℉ |
℃ | |
Grade 1 |
-50 |
-45 |
Grade 3 |
-150 |
-100 |
Grade 4 |
-150 |
-100 |
Grade 6 |
-50 |
-45 |
Grade 7 |
-100 |
-75 |
Grade 8 |
-320 |
-195 |
Grade 9 |
-100 |
-75 |
Grade 10 |
-75 |
-60 |
力学性能
标准 |
牌号 |
抗拉强度(MPa) |
屈服强度(MPa) |
伸长率(%) | |
纵向 |
横向 | ||||
ASTM A333 |
Grade 1 |
≥380 |
≥205 |
≥35 |
≥25 |
Grade 3 |
≥450 |
≥240 |
≥30 |
≥20 | |
Grade 4 |
≥415 |
≥240 |
≥30 |
≥16.5 | |
Grade 6 |
≥415 |
≥240 |
≥30 |
≥16.5 | |
Grade 7 |
≥450 |
≥240 |
≥30 |
≥22 | |
Grade 8 |
≥690 |
≥515 |
≥22 |
| |
Grade 9 |
≥435 |
≥315 |
≥28 |
| |
Grade 10 |
≥550 |
≥450 |
≥22 |
| |
Grade 11 |
≥450 |
≥240 |
≥18 |
|
化学成分
标准 |
牌号 |
化学成分(%) | ||||||||||
C |
Si |
Mn |
P |
S |
Cr |
Ni |
Cu |
Mo |
V |
Al | ||
ASTM A333 |
Grade 1 |
≤0.30 |
|
0.40-1.06 |
≤0.025 |
≤0.025 |
|
|
|
|
|
|
Grade 3 |
≤0.19 |
0.18-0.37 |
0.31-0.64 |
≤0.025 |
≤0.025 |
|
3.18-3.82 |
|
|
|
| |
Grade 4 |
≤0.12 |
0.18-0.37 |
0.50-1.05 |
≤0.025 |
≤0.025 |
0.44-1.01 |
0.47-0.98 |
0.40-0.75 |
|
|
0.04-0.30 | |
Grade 6 |
≤0.30 |
≥0.10 |
0.29-1.06 |
≤0.025 |
≤0.025 |
|
|
|
|
|
| |
Grade 7 |
≤0.19 |
0.13-0.32 |
≤0.90 |
≤0.025 |
≤0.025 |
|
2.03-2.57 |
|
|
|
| |
Grade 8 |
≤0.13 |
0.13-0.32 |
≤0.90 |
≤0.025 |
≤0.025 |
|
8.40-9.60 |
|
|
|
| |
Grade 9 |
≤0.20 |
|
0.40-1.06 |
≤0.025 |
≤0.025 |
|
1.60-2.24 |
0.75-1.25 |
|
|
| |
Grade 10 |
≤0.20 |
0.10-0.35 |
1.15-1.50 |
≤0.03 |
≤0.015 |
≤0.15 |
≤0.25 |
≤0.015 |
≤0.50 |
≤0.12 |
≤0.06 | |
Grade 11 |
≤0.10 |
≤0.35 |
≤0.6 |
≤0.025 |
≤0.025 |
≤0.50 |
35.0-37.0 |
|
≤0.50 |
|
|
GB17395-1988无缝钢管允许偏差
12Cr3MoWVSiTiB钢管12Cr3MoWVSiTiB化学成分
牌号 |
化学成分(质量分数)(%) | ||||||||||||||
C |
Mn |
Si |
Cr |
Mo |
V |
Ti |
B |
W |
Ni |
AI |
Nb |
N |
S |
P | |
≤ | |||||||||||||||
12Cr3MoWVSiTiB |
0.09-0.15 |
0.50-0.80 |
0.60-0.90 |
2.50-3.00 |
1.00-1.20 |
0.25-0.35 |
0.22-0.38 |
0.005-0.011 |
- |
- |
- |
- |
- |
0.030 |
0.030 |
12Cr3MoWVSiTiB力学性能
牌号 |
纵向力学性能 |
横向力学性能 | ||||
拉力强度MPa |
屈服点MPa |
伸长率(%) |
拉力强度MPa |
屈服点MPa |
伸长率(%) | |
12Cr3MoWVSiTiB |
610-805 |
440 |
16 |
- |
- |
- |
Gr.6无缝钢管
1.低温钢管、低温管ASTM A333 GR.6/AMSE SA333 GR.6规格
Φ762mm以下
2.化学成分
标准:ASTM A333 Gr.6/ASME SA333
Gr.6化学成分(%) | ||||
C |
Mn |
P |
S |
Si |
≤0.30 |
0.29~1.06 |
≤0.025 |
≤0.025 |
≥0.10 |
3.机械性能及冲击温度
抗拉强度(MPa) |
屈服强度(MPa) |
最小平均 缺口冲击值(J) |
最低冲击 试验温度(℃) |
≥415 |
≥240 |
18 |
-45℃ |
4.材料产地
宝钢、成钢以及德国,日本进口
5.应用
适用于低温环境作业,能承受一定的低温冲击
您可能感兴趣的钢管知识:
GB3087与GB5310的区别
无缝钢管材质
无缝钢管规格表